What kind of vehicle are you planning of applying this on?

I think that a Nickel, Triple Chrome or Copy Chrome plate would look fantastic on some finished suspension components, but the plating would need to be fairly thick to provide maximum corrosion resistance.

A Copper plate first would provide better protection under the Nickel for sure, but the Nickel would eventually dull out and tarnish under the extremes of the weather without the third step of Chrome.

Copy Chrome would eliminate the Nickel and Chrome steps in the Triple Plate System and look just as good, but it too would have to be applied fairly thick over the Copper Plate (plating times of at least 1 hour).

Have you looked into the possibilities of Powder Coating? This is a durable coating that will withstand some pretty extreme conditions. It is also available in an almost infinite selection of colors and textures.

Also, Powder Coating is not near as time consuming as Electro-Plating.

Just a thought…

Best of luck and keep us informed.