Quote:
|
Originally Posted by chromeitout
I plan to build a 55 gal. vibratory polisher after the first of the year to polish ceramic coat and it would be a bonus to change tanks/media and be able to polish aluminum as well.
|
I was thinking about building one myself, as I want a fairly large one but wasn't sure as to the mechanics of them (as I have never seen one always polished by polisher or hand) got any ideas as to how to start.