View Single Post
  #3 (permalink)  
Old 12-20-2006, 08:42 PM
lcaswell's Avatar
lcaswell lcaswell is offline
Caswell Inc President
 
Join Date: Jan 2001
Location: Lyons NY USA
Posts: 2,352
Blog Entries: 3
lcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud of
Default Re: Zinc Plug N Plate Dark Streaks/Coverage Capacity Questions

The zinc solution will cover approx 2-3 sq ft. Immersion plating to 0.0005" would take approx 10 minutes, so expect the same, theorectically, for brush plating the exact same area with the wand.

Also, the wand in the zinc kit will wear away. When the zinc strip in the wand is gone, it's time to buy a new one.

You can't replenish Plug N Plate solutions. You'll need to buy a new bottle when it's all used up.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote