Re: Caswell's "Tinted Brass" and "Candy Gold "
they are both transparent colors
you will always see the metal below if you don't use a base coat
you'll need to coat with a chrome base first and then top it with gold or brass
to make it look more like cadmuin or zinc palting I would use a silver base instead of chrome
|