Re: fish eye any way around it ?
What you are calling fish eye is orange peel. Fish eye is caused by contamination and orange peel is the coating not flowing out. The way I deal with it is to dwell the temp that the powder starts to melt and flow for a short period of time. At times you may need to increase the coating thickness.
SS
|