Thanks, i went back and tryed to go back with 400 and then wet sanded 600. and i got the same results with the hazing. I even bought some tripoli to try and same thing. Do you guys think i need to just start over and sand everything back down and start back with 180. It seems like nothing is helping. I havent tryed the felt wheel yet, maybe i will hit it with that with the white like Jrow said and see what happens.