Quote:
|
Originally Posted by bewsted
Is it possible because i am using a drill to polish, that i actually might be getting to hot, causing the haze?? i just thought about that.
|
Nope - if anything, the slower speed of the drill is better for a final buff than a high-speed machine.
When you clean up, do you find the cleaning process making scratches? I just did a pulley where I'd get it perfect, but even gentle cleaning with microfiber cloth left marks. It's one reason people chrome plate things - it's a much harder surface so will hold a better finish.