sal1355,

It is a matter of personal preference, time and money.

Are the judges going to be looking for show quality Triple Chrome Plate on all of your misc. fasteners and such, or are they just going to look at the overall quality of the pieces in general?

A true Triple Chrome Plate is expensive to get started in and requires a lot of steps but is well worth it if that is what you require.

Copy Chrome is much safer and has a lot less headaches involved, especially when doing little parts and pieces.

A well executed Copy Chrome job looks just as good as Triple Chrome and the differences are very subtle. They would probably go un-noticed if done correctly.

I use a small Copy Chrome kit for all of my indoor and outdoor decorative items such as nut, bolts, brackets, chains, door hinges, etc. and have had excellent results with the finish quality and durability of the final plate.

In my opinion, a 1.5 or 3 Gallon Copy Chrome Kit would be perfect for your application.

For larger, more visible parts, I would recommend the Triple Chrome Plate set-up. Especially if doing actual show car pieces.

Best of luck,