Default Re: How To Powder Coating Ghost Flames

Or, 2 shades of Candy/lollypop red.

Base of chrome, bake fully
Mask, preheat to 200-250
spray light dusting of lolly
Bake for half time, to flow out
Take mask off
spray rest of lolly, full cure



The ghost flames would be a darker shade. But, because it was under cured initially, it should all flow smooth?? I have to try this.