Default Pot Metal Electroless Nickel - Suitability as finish

I am planning on nickel plating some small zinc and aluminum parts and had planned on doing the following:

1. Strike coating the aluminum parts with Zincate
2. Finish plating both the aluminum and pot metal parts using the Pot Metal Electroless Nickel kit.

Would this process work and produce acceptable results?
What is the thickness of the nickel plate that is produced using the Pot Metal Electroless Nickel kit?

I am hoping it will work as I have a very limited budget.

The total surface area of the parts is approx 2 square feet and they all have a matte finish.