Quote:
Originally Posted by mikekozura
Stripper…. OK what were you guys thinking. What’s the best stripper for powder coat.

Well , i picked up a empty steel 55-gal drum & started filling it 5-gallons at a time with paint gun cleaner AKA "Naked gun cleaner". The stuff rocks !!! will strip down a powdercoated wheel to bare aluminum in about 20-30 minutes.

One suggestion , use a good mask and good gloves when using it. Very bad for you..lol

I usually used the "aircraft" stripper, works good but the gun claener cut down on my stripping labor time by 75% !!

thanks , TIM