has any one out there used the new silvaspray. i keep having delaminating problems when i pull it from the solution. the plate sticks very well to the silvaspray but the silvaspray delaminates.

it failed on all kinds of plastics and sandblasted pot metal with body filler.

if you have it and it works for you let me know what you think.

thanx.bondo