View Single Post
  #5 (permalink)  
Old 01-13-2007, 03:16 PM
neeraj_bapat neeraj_bapat is offline
Newbie
 
Join Date: Jul 2006
Posts: 5
neeraj_bapat is on a distinguished road
Default Re: Plating Surface Quality for Plastics

I mistakenly typed 2 am/in2; I am using CD of 0.2 a/in2.

I want to use copper as a final layer of plating..What should be done to avoid discoloration of plated copper. it turns dark red in patches upon washing with distilled water.