I have done my mx bike in swb as well. they hold up just fine, however, you are going to get some scratching around the bead where you use your tools to put the tires back on. I pc'd my tire tools to help with this and it seems to have helped. I ended up with only 2 minor scrapes on mine. If you are using a hobby gun like me, definitely heat it up to 150-180 to shoot the clear. Atleast thats how i did mine and it worked out extremely well.