Default Re: can you polish copy chrome??

Just a thought.

Remember that excessive buffing will make the underlying plastic and SIlvaspray soft, and the electroplate will blister, so try to ge this as smooth as possible BEFORE you plate it. Then you will need very little buffing.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote