Quote:
|
Originally Posted by boston_jake01
I was wondering if there is any quick way to remove adhesive from fenders?
I am sanding them for repaint and was trying to wet sand them off but it is taking forever.
Thanks
|
Have you tried Lacquer thinner, Acetone or MEK?