The pot metal nickel kit isn't designed to be used as a final plate.

You'd be better off getting a Flash Copper Kit and a Nickel Plating Kit.

If finances are a concern, the regular plating kits are much cheaper to operate than electroless systems.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote