Default Re: cheap excellent material for oven walls

I've been up to 250 so far. Havn't got the doors sealed and need 2 more elements to get to cure temp. It seems to take a while to get up to temp. Cause you are basically heating up rock. But, it also keeps heat nice. OPen doors, long enough to simulate loading pieces, doesn't drop as much as my small oven
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"