I powder coated these heads and I also polished the edges.
I first polished the edges and then taped the edges (whichwas a pain in the ass ) then I pwder coated them, after it cool down I removed the tape and found that the powder got in some area I taped I had to repolish the edges and when I ran the buffing wheel to close and hit the coated areas it turned black ( Iguess from burning it ) the picture is not to good. I am really anal and dont like to see any pwder where it should be. any Idea on how to do this better?