I just powder coated my oil pan using a hardware store variety quartz heater. It worked very well. Since the oil pan is only coated on the outside, I used my heat gun on the inside of the pan to get the nooks and crannies up to temp without overheating the large flat panels. Worked great. I was impressed how easy it was.
Hemi-T
|