Exclamation thin areas on bike frame using metallic

HELP !!!!!!!! I just shot a motorcycle frame for my first customer and even though I looked over the frame really well before putting it in the oven I have several areas that are thin or have no powder at all. The powder is champagne metallic that I bought directly from Tiger as Caswell didn't carry it.

Can I touch up the areas without messing up the rest of the frame? I am not sure if I have enough powder left to reshoot the whole thing, nor do I have the time to take the frame back down to bare metal.

I tired to color sand a test piece that I shoot two coats onto and it didn't turn out well as a shade difference was noticable at the edge of the two coats.

Thanks in advance for any help.