Default Re: Just got my greasless!!!!

arrrrggggh, wish i had seen this before i went to bed, i opened one this morning and had a little go with it, spun it up on my felt bobs and covered it, dried it with hairdryer and had a go, very impressed. Was put in the shed but its like a firdge in there anyway

just gotta buy some smaller felt bobs now as the ones i just ordered are too wide to get into the places i need, typical. Got work tonight but will be having another go at it tommorow.

Can you heat up em with a hairdryer to make them melt a bit so u can just dunk the felt bobs in a runny gue?

How about loading up loose mops? is that possible? Thinking along the lines of loose mops get into more creveses etc so maybe they would sand in more creveses?

Last edited by Tng21; 01-26-2007 at 12:51 PM.