I have 4 elements like that in my small oven. They are used alot in industry as worker area heaters. Mine are 3 feet long, approx 7500Watts combined. They work pretty good. I have them mounted in a 4'x3'x16" oven

BTW, nice CNC. I have one here too, although it's a little smaller