Join Date: Jun 2003
Posts: 20
The kits arrived yesterday. Unfortunately, it appears the instructions for the Pot Metal Nickel Kit have been ommited from the 5th edition plating manual.
Could you send me instructions via email or a message on these forums
Thanks!