Default Re: Black oxide problems

Quote:
Originally Posted by destroyer125
.... I am using the stainless steel blackener....

Did you ever get the 370 to work? There is little or no information about the 370, not even a tutorial. I have tried just about everything including the countless one line instructions via email from tech support and the $320(4x$80ea) worth of barrels I've ruined really sucks(and I don't mean cosmetically either, they cannot be used because they are etched VERY badly). I even purchased some industrial grade muriatic acid(80%) as suggested and nothing seams to keep the parts from looking like they have leprosy(like your photo of the screw) or to keep from just wiping what little spots of black there is off with a rag?

TIA