Thread: problems
View Single Post
  #3 (permalink)  
Old 01-29-2007, 02:45 PM
krymis krymis is offline
Amateur Metal Finisher
 
Join Date: May 2006
Posts: 82
krymis is on a distinguished road
Default Re: problems

I shot the blue cold because of the polished letters and fins. I wiped the powder off with a damp spong. Usually i shot the candies hot at about 150-180.