Default Electroless Plating on Chainmail Pieces

I am into Chainmail Fashion Jewelry Making. I use stainless steel rings. I want to add more luster to stainless steel. I tried Electro-Decorative Chrome plating. But, the electrical distribution was not even among the interlocking rings which results to an uneven plating.

I read about your electroless nickel and electroless chrome. Can we combine it to achieve the effect of electro-decorative chrome?

Do you have vibratory tumbler abrasive compounds? for surface preparation? nickel buffing? chrome final buffing?