Mine did the same thing. It was shot on a LT1 intake. I blasted it, cleaned it off, heated it at cure temp for 30min, and shot it while it was still warm (I don't know the exact temp cause i don't have a laser temp gun). I shot the blue over bare metal. The guy said it did the same thing with slight taps from a socket it chipped. I guess the part didn't get up to cure temp for long enough? Before I shoot it again I am going to get a temp gun! Any other advice, besides what has been said? Thanks!