Thread: Stripper
View Single Post
  #23 (permalink)  
Old 01-31-2007, 09:01 AM
JTW37's Avatar
JTW37 JTW37 is offline
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 600
JTW37 is an unknown quantity at this point
Exclamation Re: Stripper - New Product!?

Okay, after reading the posts about the stripping of powder coat, I did some searching. First off I found the Kleanstrip locally. But after talking to a young lady about this cleaner, she told me of a stripper that they have just gotten in within the last month or so and that I should give it a try. So, I will get some today and report back on it. She claims that the demo that she seen, was absolutely awesome to see. According to her, it just lifts powder right of of the item coated. It's a bit pricey, but if it will do what most can't, I game. One of the major differences is that it is NOT harmful to you or your skin and IS biodegradable. Says that they have been selling quit a bit of it.

I will report on this, hopefully tonight after I get it and test it, as I have a tank that refuses to come completely clean, even with the Aircraft stripper. So, stayed tuned.
JT