Default silver on silver?

I have a musical instrument mouthpiece that is silver plated brass. I want to increase the diameter of the shank (end that goes into the instrument) by approximately .001". Is it possible, using the Plug and Plate to silver plate onto an existing silver plate, or do I need to use gold or some other metal? Also, does anybody know what range of thicknesses can be achieved by doing so? I need to get about .0005" of plating on both sides of the shank. I have tried using the rub-on Silverplater, but have not been able to get a measurable thickness difference (silver on silver).

I am new here, and new to plating. Thanks.

-Craig
Reply With Quote