Re: couple of dumb newbie questions
1) It is possible to use a battery charger but the anodized layer will not be of very high quality. So the anwser to your question is yes, but if you are only going to anodize one part the trouble is far greater than it is worth.
2)Estamate the area by looking at the lever like parts of a retangle or a cube and just watch your amps going to the part.
|