Okay, didn't get the stripper going until later today. Well that's not totally true. I did put some on it. But like a lot of us and the guy thing, I didn't RTFB. I didn't stir it up before using. And I only applied it to a small area. Anyway, on that spot it lifted of in on piece, so wonder what will happen now that I have read the instructions on the container.

I put it on, but was busy working on my oven and doing a small powder job, so didn't get back to it. Will check it in the morning. They said I could leave it over night and it would still be good in the morning. That part is true.

Stay tuned. I will have a report tomorrow sometime.