Man am I ever sick and tired of that kitchen oven. Every time I attempt to put something in it after spraying, I either touch it or it bumps somewhere inside of the oven. Sure glad I started building my BIG oven. Can't wait till I get that done.

Mine is going to be 3'x3'x6' standing, when it's done. Am planning on three 2700 watt elements, the contactor that most of you are using, with a Berger-Coleman controller. Are the elements going to be enough or should I add another one?

Also want to have lighting in the oven and a door glass. I have noticed that many do not have this. Is it necessary to have the glass or no? Some of the powder says after it flows all over then lower the temp. How else would you know, without opening the door?