I never stop at 360 grit. I use 400 and then emery on stainless, and on aluminum, since it's so easy to sand, I go way up, to sometimes 1000. Then I start with tripoli, which is 1200. Some alum. seems to not like tripoli, but most does okay. To go from 360 to white is just too big of a jump. It would take forever to get the 360 scratches out with white compound on a Dremel.