Container choices for Nickel Acetate sealant
I want use a container and heat it on top of a portable electric range for nickel acetate.
I would like to avoid using ceramic heaters if I can.
I know I can't use stainless steel or alum, but can I use Pyrex or a steel pot coated with porcelain enamel on the inside of the pot?
Also, does the nickel acetate discolor my clear ano parts?