Default Re: How do I polish expanded aluminum??

lostinnd,

Anything that you use is going to get pretty beat up. I would lay the expanded aluminum on a flat surface, fasten it down as securely as you can. I would then try using hard felt buffs. The only other thing I can suggest if that doesn't work out would be to farm it out to someone that has a tumbler that your aluminum will fit into.

John