Thanks sswee and sage,
I didn't think the stainless was helping things but I didn't really know what else to use. I am going to try to find some aluminum screws until I can get some titanium ones.
As far as the amperage settings go I'm a little confused there. On the 720 calculator there are boxes to input data sqin, mils, and current density. Since I am doing LCD shouldn't that be between 4.5 and 6 amps? If so, then I should have had the current set to 2.32 and done it for 84 minutes? I saw the 6 in the top box and had a brain fart and set my current to 5 not 2.32. I have the Caswell rectifier so fine tuning the current draw is a little tougher and the voltage is not adjustable. Maybe I'm really confused and need a lot more help than I think I do. I guess I am going to strip it and try again. Comparing it to what is on the car now it looks really bad.
Thanks for the input.