Originally Posted by sage
Sorryto butt in the thread but I've never done masking. When you guys say "rubber cement" do you mean regular contact cement or something else?

Sage
Not contact cement... it sticks tenaciously.
No, I mean the cheap school-grade rubber cement for crafts, etc. Elmers makes some, and it comes in a small brown bottle in the pens/paper/school supplies section of Walgreen's, etc.
After sealing, it will easily rub off. Just make sure it's completely dry before going into any solutions.
__________________
Specializing in anodized graphics in Paintball guns.