I was able to find some aluminum screws this morning, they will do until I can get some Titanium ones. I really have no idea what Ford used when making these parts, but after polishing they do not turn black if left sitting. I also hope that they did not use Electopolishing or Bright-Dip when finishing them. That is going to create another host of issues if they did.

Do you think that the bath may be contaminated becuse of the stainless and should I switch it out? I have read other post where people had the same problem, and it seemed that after another run in the bath things were fine. Just wondering.....