Guys I would question using that type of charger. It has Input/output opposite connecting protection fuction for one. I don't know how it will "see" anodizing. I know not to use a automatic battery charger because once it sees any drop it will cut off I would think also with this charger it would do the same. I think it's onboard computer is going to outsmart you while trying to anodize with it.
I just ran a bunch of classic BMX bike parts for a fellow and the color gold you want is the Golden Orange.

Later,
Tim