Caswell sells a good assortment of felt bobs. Just look in their on line catalog.

For sanding, I use two things. I use a die grinder with Roloc disks. You can get 1.5 inch disks. I don't know about 1 inch discs. For finish sanding I use a Chicago Pneumatics air sander, model 7201P. It runs at 2500 rpm. It come with 3 inch pads, but I make my own pads to fit it, whatever size I need. Tool Warehouse seems to have the best price. That's where I bought mine. If I have one tool I dearly love, it's that one.

Richard