It depends on where the part is placed and the stir speed. If the part is magnetic (steel), needs to be placed as far from the stir bar as possible, to minimize the effect of the magnetic attraction. The stir speed should be enough to agitate the solution to dissipate the hydrogen gas from the surface of the part (or oxygen gas if anodizing), not so fast that it creates a whirlpool.