I would let gravity work for you & place the elements on the bottom. yes use a fan to circulate * equalize the temp. a hogh temp. blower with a low cfm would suffice for you, something like 100cfm would be plenty. place the thermocouple somewhere in the middle of the height of the oven. some folks vent their ovens & some don't. u can rig up a vent with parts from the Home Depot for ~ $5.