Just thought I would post about my oven.
It is made from 2x2 scrap tubing. Sheet metal is 28 gage. Won't use that again. To flimsy. It's a good thing I put it on a frame or I would have a wondering wiggling oven.


Measures 3x3x68" on the inside. 40" x 39" x 72" outside. I wanted 36x36 on the inside. Need to do wiring and setup a fan. Have double doors, so it wouldn't tip when the door was opened. Besides, I like to double door idea.

Have to find oven door glass and lights next, so I can see inside. Anybody know where I can get the glass cheap?