Re: Cerakote burning/flaking off??
Process was exactly as described on your site.
Blast surface
Pre-bake at 450 for 30 min to evaporate any oils, moisture
Spray cold
Let air dry fro 20 min
Back in oven, 250* approx for 20 min to finish drying coating
Then turn oven up to 525 a,d bake for an hr once it's at temp
It's cerakote Chromex. not the colored stuff.
|