Quote:
Originally Posted by itsallgood
I just finished building my oven, I'll post pictures soon.

How long does your oven take to reach 350* once you hit the power and how big is the oven?

The oven i built is 4x4x6 and From dead cold 40* it takes about 17 min to reach
350*. About 23 min to reach 450*.