Default Re: what went wrong?

Quote:
Originally Posted by acidrain
I'm not going to convert your cm to in, but one thing that jumps out is the cool temp dying... the dye has to be heated to 140F, or it's not going to work.
One of the dye-baths was warmed up, but I didnīt measure the temp. Anything else it might be? Is it harder, in general, to get brighter colors right? What about the PS? I know itīs not optimal, but will it work?

Epreciate the help!

Last edited by dewil; 02-13-2007 at 03:25 AM.