Default Re: what went wrong?

Quote:
Originally Posted by acidrain
Tim is descibing the "let-er-fly" method. Caswell does not subscribe to that method, and neither do I.
Only with carfully controlled perameters can you expect repeatable results.
All of your tank temperatures are critical, especially the ano tank... just a couple of degrees one way or the other drastically changes the resistance. I suggest 68-70F.

I have ordered a CC powersource now so I can have full control of the power. I had no idea that the bath-temp was so critical, it must have been way off since my line is in a pretty cold garage! Ill see if I can find some descent heaters!
Thanks