Default Re: Zinc Plating & Amps Query

Cahrles:

Size disparity between parts is irrelevant. You simply need the total surface area of all parts combined.

eg, take a 9" part & a 1" part together. The 9" part will attract 90% of the current, the 1" part 10%. Each will get the same ASI.

You'll likely never need more than the 5-7 volt setting, as long as it allows you to set the appropriate current.

Sean