Re: What kit to use
In this case I would not use the pnp it will not give you the thickness and coverage necessary
for this typ of project. I have used the copy chrome and had it installed next to many triple chrome items and have not had a problem with color difference. This piece you are talking about should be dipped for maximum coverage